wangliang
Ask a question. This is a fillet weld on the drum. The working pressure of the drum is 4.3..
海阔天空
The external pressure vessel is used for hydraulic pressure test...
TuKai
Excuse me, the medium temperature is -25°, the atmospheric tank, lined inside. The shel..
hao先生
Ask me if ammonia belongs to the first group or the second group. According to the volume ..
阳光boy
Are the butt welds of the heat exchanger tubes 100% flaw detection?..
光头强
Parents, the height of the welding feet of the semi coil tube
[this_is_pic_0..
啊呀呀
Do Q245R heat treatment require special specification for normalizing plate?
Request..
啊呀呀
The maximum thickness of the heat treatment report is the maximum thickness of the weld.
一路向东
Non standard flange, if seal is not required, what specifications are there in size only, ..
是董小姐呀
The manhole standard is Q345R material
Can it be replaced by the 20# tube?